■ slag remover
It is used to remove slag from the surface of casting solution of foundry plant and iron and steel plant, ensure that the casting solution does not contain impurities, prevent oxidation, and can be used as heat preservation material, so it has excellent performance, so it is very suitable as slag remover.
[Characteristics]
The slag and foreign matters mixed in the casting solution can be collected, and the residue can be removed once.
When pouring into a small pot, it can prevent reflection and refraction for easy operation.
The surface of casting solution is evenly spread, which can gather slag and foreign matters to prevent mixing into the product during pouring.
● does not change the composition of the casting solution.
It is easy to operate and will not raise dust.
Compared with straw ash, rice husk is more convenient for management and storage, and does not occupy space.
It is not affected by season, and can be supplied at any time without fire risk.
It is produced by the factory, and the quality and quality are uniform.
[usage]
1. use a spoon, shovel and so on to take "Ishikawa light stone" near the casting solution and spread it.
At the same time, a film is formed on the surface of the solution, which is bonded with the slag to form an expansive body.
Then, the proper rod-shaped tool is used to pick up the expansion body to ensure the clean casting liquid.
2. According to the type of solution, the capacity of taking pot and dissolving furnace, the purpose of use and the amount of use are different. In general, the usage of "Shichuan light stone" is 0.3-0.6 liters per ton of casting liquid.
3. Avoid spreading as much as straw ash.
[list of various products]
| |||||||||||||||
|
No.3 | Purpose | Stainless steel, spheroidal graphite casting, ordinary casting | |
Temperature | 1500℃~1600℃ | ||
Dissolving furnace | Electric cupola | ||
Grain size | order | 14~28 | |
mm | 1.18~0.6 |
No.4 | Purpose | Spheroidal graphite casting | |
Temperature | 1300℃~1500℃ | ||
Dissolving furnace | Electric cupola | ||
Grain size | order | 28~48 | |
mm | 0.6~0.3 |
No.5 | Purpose | Spheroidal graphite casting | |
Temperature | 1300℃~1400℃ | ||
Dissolving furnace | Electric cupola | ||
Grain size | order | 48~60 | |
mm | 0.3~0.25 |